Skip to main content
. Author manuscript; available in PMC: 2014 Sep 20.
Published in final edited form as: ACS Chem Biol. 2013 Jul 26;8(9):2063–2071. doi: 10.1021/cb400258d

Figure 5.

Figure 5

Effect of receptor density on the binding kinetics of G5-MTXn (n = 5, 10). (A, B) Each plot shows average traces of sensorgrams (n = 3) obtained from the dendrimer injection at the variable level of FBP density. (C) A plot of fractional desorption of G5-MTXn in response to variation in FBP density (n = 3; mean ± SD).