Skip to main content
. Author manuscript; available in PMC: 2013 Oct 8.
Published in final edited form as: Biomaterials. 2009 Feb 23;30(17):3058–3067. doi: 10.1016/j.biomaterials.2009.01.054

Figure 5.

Figure 5

Characterization of hMSC. Deposition of GAG (A) and calcium (B) in passage 2 and 3 hMSC (P2, P3) in pellets cultured in either control, osteogenic or chondrogenic medium for 3 weeks. Flow cytometry with positive expression of the surface antigen CD 105 (C) and negative expression of CD34 (D) and CD 31 (E) on P2 hMSC.