Figure 4. Critical adhesion energy (Gc) in air with a 20% relative humidity and in water at 21°C for (a) interface between thermally grown SiO2 and Ti, Ni and Cu, respectively and (b) interface between Ni and various SiO2, including spin-on-glass, soda-lime glass, native SiO2 and thermal SiO2.