KSL-W microsphere properties.

Formulation Surface morphology Yield (%)  KSL-W content (%)  Loading efficiency
   (%)
 average size (µm)
   n = 30
% Release at 150 hours
In PBS In Gel
A Spherical,
high surface porosity
75 17 68 46.4 ± 17.9 52.0 ± 2.5 64.4 ± 2.7
B Spherical,
high surface
porosity
84 19 77 25.8 ± 14.1 74.8 ± 2.3 76.3 ± 1.2
C Spherical,
high surface porosity
68 20 78 40.0 ± 12.8 53.3 ± 4.5 68.3 ± 3.6