Table 2.

Percentages of failure modes after microtensile test. T0, T6 and T12 indicate specimens that were tested after storage for 24 h, 6 months or 12 months, respectively. Fractures were classified as: A, adhesive; CD, cohesive failure in dentin; CC, cohesive failure in resin composite; M, mixed failure.

Adhesive system Adper Scotchbond 1XT XP Bond
Storage time T0 T6 T12 T0 T6 T12
0.2% chlorhexidine 30% A
70% M
[5/163]
30% A
5% CC
65% M
[5/154]
30% A
70% M
[6/161]
40% A
5% CD
55% M
[7/158]
35% A
65% M
[6/154]
30% A
10% CD
60% M
[4/159]
2% chlorhexidine 35% A
10% CD
55% M
[8/167]
35% A
5% CD
60% M
[5/162]
50% A
5% CD
45% M
[7/149]
45% A
55% M
[4/163]
30% A
10% CC
60% M
[5/162]
40% A
15% CD
45% M
[7/164]
Control group 35% A
65% M
[6/159]
30% A
10% CC
60% M
[9/172]
35% A
10% CD
55% M
[5/167]
35% A
65% M
[6/154]
35% A
5% CD
60% M
[7/165]
35% A
15% CC
50% M
[6/158]

[number of premature failed sticks/number of intact sticks tested].