Skip to main content
. 2013 Sep 17;13(9):12467–12481. doi: 10.3390/s130912467

Figure 4.

Figure 4.

Response of the sensor element using Co3O4 powder during exposure to NO2 (0, 0.5, 1, and 5 ppm) in air at (a) 100 °C and (b) 200 °C. The inset shows the relationship between the sensor response and NO2 concentration.