. 2013 Oct 10;14(10):20189–20203. doi: 10.3390/ijms141020189

Figure 6.

Figure 6

Weight loss of the examined samples as a function of degradation time: (a) PLA; (b) PBAT; (c) PLA/PBAT (80/20, w/w); (d) PLA/PBAT/ADR (80/20/1, w/w) and (e) PLA/PBAT/HDE (80/20/1, w/w).