Skip to main content
. 2013 Nov 4;2013:465086. doi: 10.1155/2013/465086

Figure 2.

Figure 2

An optical image of the fabricated 0.5 wt.% MWCNT/45S5 Bioglass composite scaffolds before and after heat treatment at 900°C, which shows the shrinkage of samples.