Tabletability (Tensile Strength in MPa) of Selected Silicates Blended with 20% w/w MCC (Average of 2 Determinations)

Silicate used (+20% w/w microcrystalline cellulose) Tensile strength (MPa) at different compression pressure
50 MPaa 150 MPaa 250 MPaa
Aerosil® 200 0.1 0.4 Broken
Neusilin® UFL2 1.4 4.4 5.0
Neusilin® US2 1.2 5.3 4.6
Sipernat® 22 Broken 0.6 1.2
Sylysia® 350 0.1 0.9 Laminated
Zeopharm® 600 0.6 5.5 5.0