Mean ± S.D. Range Average CV (%) ICC
Yield strain (%) 0.78 ± 0.05 [0.70, 0.87] 1.01 0.988
Yield strength (MPa) 3.09 ± 1.01 [1.62, 5.11] 3.65 0.995
Ultimate strain (%) 1.35 ± 0.28 [0.90, 1.95] 3.68 0.987
Ultimate strength (MPa) 3.48 ± 1.05 [1.75, 5.51] 3.42 0.994
Modulus of resilience (kPa) 14.30 ± 5.39 [6.83, 25.85] 4.19 0.996
Toughness (kPa) 32.77 ± 12.22 [16.09, 60.22] 5.62 0.986