Table 2.

Total ester conversion with supported Pd on two different morphologies of SBA-15

Catalyst BET surface area (m2/g) Pd dispersiona (<) Total ester conversion (<)
N1
482.2
39.2
95
S1 431.9 18.5 94.3

aMetal dispersion determined by H2 pulse chemisorptions.

N1: 3.8 wt< Pd/SBA-15-necklacelike.

S1: 3.8 wt< Pd/SBA-15-spherelike.