Skip to main content
. 2013 Sep 28;6:284. doi: 10.1186/1756-3305-6-284

Table 1.

Composition and physicochemical characterization of deltamethrin-loaded mosquito repellent patches

Formulation batch EC: PVP-K 30 Weight variation (gm) Thickness (mm) Surface area (cm2) Moisture uptake (%) Moisture content (%) Deltamethrin content (%)
A1
1:2
0.47 ± 0.07
0.42 ± 0.03
14.51 ± 0.68
7.31 ± 4.33
4.50 ± 0.60
50.35
A2
2:1
0.48 ± 0.06
0.41 ± 0.01
13.84 ± 0.66
4.67 ± 2.66
3.13 ± 0.10
75.76
A3
3:0
0.46 ± 0.10
0.51 ± 0.01
14.30 ± 1.41
3.42 ± 2.66
2.60 ± 0.25
77.60
A4
0:3
0.54 ± 0.06
0.57 ± 0.01
14.09 ± 1.68
8.92 ± 5.79
5.52 ± 0.43
62.05
A5 1.5:1.5 0.46 ± 0.04 0.35 ± 0.01 13.64 ± 1.37 6.23 ± 1.57 3.18 ± 0.11 66.41