Experimental material parameters of SMA wires.

Martensite R-Phase Austenite
TCR: αi (μΩcm·°C−1) 0.08 −0.05 0.05
SCR: βi (μΩcm·°C−1) 0.05 0.04 0.04
Stress on temp.: Ci (MPa·°C−1) 3.68 - 6.06
ER at zero stress and T0i: p0i0 (μΩcm) 100.5 104.2 95.2
T0i (°C) 34 58 79