Skip to main content
. 2013 Nov 8;13(11):15324–15347. doi: 10.3390/s131115324

Figure 11.

Figure 11.

Thermoelectric output of a In2O3:ITO 95/5 thermocouple tested after a 5 h, 500 °C nitrogen anneal and 2 h, 1,000 °C air anneal. Note the stability of this all-ceramic thin film thermocouple over the testing period. A drift rate of 2.74 °C/h was observed.