Figure 22.

Figure 22.

Isothermal constrained shrinkage ((V0−V)/V0) of In2O3 films prepared in Ar (blue square), Ar/O2 (green circle) and Ar/N2 (red triangle) plasmas at 1,300 °C as a function of time.