Skip to main content
. 2013 Nov 8;13(11):15324–15347. doi: 10.3390/s131115324

Figure 9.

Figure 9.

Thermoelectric output of a Pt:ITO 90/10 thermocouple tested after a 5 h, 500 °C nitrogen anneal and 1 h, 1,000 °C air anneal. Note the improvement in signal drift and device durability over the same testing period. The film thickness was 6 μm. A drift rate of 2.64 °C/h was observed.