Scaffold Porosity, volume % Pore size (average), μm
0 P 60±5 110–280 (200)
0.1 P 62±6 70–150 (110)
0.3 P 63±5 50–250 (160)

Notes: 0 P, 0.1 P, and 0.3 P represent the scaffolds prepared from 0%, 0.1%, and 0.3% (w/w) poly(3,4-ethylenedioxythiophene) poly(4-styrene sulfonate) in the mixture of 10% (w/v) gelatin and 30% (w/v) bioactive glass nanoparticles.