Skip to main content
. 2014 Jan 9;4:3620. doi: 10.1038/srep03620

Figure 3. (a) typical TEM graph of the MDZ-C sample; (b) and (c) SAED patterns of 18R-LPSO phase along [1000] direction and Mg matrix in (a), respectively; (d) eutectic phase in the MDZ-C alloy; (e) SAED pattern of eutectic phase along [114] direction in (d); (f) TEM graph of the MDZ-545 sample; (g) SAED pattern of 14H-LPSO phase along [1000] direction in (f).

Figure 3