Figure 4.

Figure 4

SEM images of Ti-discs prior to incubation in SBF (x 5,000) (a) B = blasted; (b) AH = alkali and heat treated; (c) AO = anodically oxidized; (d) HA = hydroxyapatite coated; (e) B- = blasted titanium incubated in non laminin containing SBF. The bar presents 10 µm.