Failure temperature after PAV of SBS modified asphalt soaked in saline water.

SBS modified asphalt 0%
0 d
0.3%
7 d
0.3%
15 d
1%
15 d
1%
30 d
3%
1 d
3%
30 d
5%
1 d
5%
7 d
Failure temperature (°C) 78.70 80.33 80.28 79.27 79.23 79.82 78.90 79.61 81.43