Skip to main content
. 2013 Oct 11;38(1):47–53. doi: 10.1007/s00264-013-2113-0

Fig. 4.

Fig. 4

Two exemplary X-rays before testing (a left) and after failure (a right) the white dots mark the points for X-ray evaluation. Mode of failure with plate bending in the LAP group (b left row) and blade bending with cracks nest to the screw hole for the non-contact bridging plate (b right row)