Skip to main content
. 2013 Nov-Dec;21(6):590–596. doi: 10.1590/1679-775720130255

Table 2.

Shear bond strength (MPa) mean values (±standard deviations) of resin composite to sandblasted cpTi surfaces with metal primers after 24 h of water storage (T0) or after thermocycling (T1). Means followed by the same capital letters in a column and lower case on the lines do not differ significantly by the Tukey test (α=0.05)

Metal primers Storage condition
T0 T1
MPP 8.4(1.3)Ba 8.1(1.0)Ba
OP 10.4(2.2)Aa 12.1(1.9)Aa
S 9.6(1.2)Ba 9.1(0.9)Ba
TL 10.6(1.9)Aa 10.2(1.4)Ba