Skip to main content
. 2014 Jan 9;5:26–35. doi: 10.3762/bjnano.5.3

Table 1.

Thickness measurements of TMMH on gold substrates.

AFM protocol TMMHa thickness (nm) Example

Time-lapse AFM study, upright adsorbates on gold 1.0 ± 0.2 Figure 2
Nanoshaving of mature SAM of TMMH 1.0 ± 0.2 Figure 4
Nanografted ODT within TMMH matrix SAM 1.2 ± 0.2 Figure 5
Nanografted MUA within TMMH matrix SAM 1.0 ± 0.2 Figure 6
Nanografted TMMH within dodecanethiol SAM 0.7 ± 0.3 Figure 7

aThe error is estimated to be at least 0.2 nm from the thickness of a gold step.