(a) Topographic surface images of PCL films observed by AFM at 25 °C (left) and 45 °C (right); (b) 3D AFM images of 70/30 PCL film observed at 25 °C (left) and 45 °C (right). All images were obtained in the 20 μm × 20 μm scan range.