Skip to main content
. Author manuscript; available in PMC: 2014 Oct 22.
Published in final edited form as: ACS Nano. 2013 Sep 6;7(10):8849–8856. doi: 10.1021/nn403302s

Figure 3.

Figure 3

Peak fraction of the total CNT area for six temperature steps (bars) and time required for 50% mass loss (solid diamonds connected by a line) for a W-CNT under oxidizing conditions after treatment with the chemical digestion reagents. Grey shaded area is the functionalized W-CNT after treatment with Solvable.