. 2014 Feb 5;4:3978. doi: 10.1038/srep03978

Figure 5. Photocatalytic performances of Ta3N5-Pt cloth.

Figure 5

The degradation efficiency of (a) MB aqueous solution (10 mg L−1, 60 mL) and (b) 4-CP aqueous solution (1.28 mg L−1, 60 mL), versus the exposure time under visible light irradiation (λ > 400 nm), in the absence of photocatalyst and in the presence of SiO2–Pt powder, bulk Ta3N5 powder, bulk Ta3N5-Pt powder, Ta3N5 cloth or Ta3N5-Pt cloth. (c) DMPO spin-trapping ESR spectra recorded at ambient temperature in the aqueous solution with Ta3N5 cloth for DMPO-·OH under visible light irradiation (λ = 532 nm). (d) Cycling photocatalytic test of Ta3N5–Pt nonwoven cloth (20 mg).