Figure 3.

Figure 3

Low magnification scanning electron microscope (left panels) and energy-dispersive X-ray spectrometer micrographs (right panels) of resins filled with MI-POSS.

Abbreviations: EDAX, energy-dispersive X-ray; MI-POSS, methacryl isobutyl polyhedral oligomeric silsesquioxanes; MI1, resin with 1 wt% of methacryl isobutyl polyhedral oligomeric silsesquioxanes group; MI3, resin with 3 wt% of methacryl isobutyl polyhedral oligomeric silsesquioxanes; MI5, resin with 5 wt% of methacryl isobutyl polyhedral oligomeric silsesquioxanes; MI10, resin with 10 wt% of methacryl isobutyl polyhedral oligomeric silsesquioxanes; SEM, scanning electron microscopy.