Skip to main content
. 2014 Jan 6;14(1):868–876. doi: 10.3390/s140100868

Figure 2.

Figure 2.

Figure 2.

(a,b) SEM images of unstrained (0%) and strained (400%) MWCNT-coated NR samples; (c,d) SEM images of unstrained (0%) and strained (400%) graphite-coated NR samples.