Skip to main content
. Author manuscript; available in PMC: 2014 Feb 20.
Published in final edited form as: Small. 2010 May 21;6(10):1082–1086. doi: 10.1002/smll.200901538

Figure 4.

Figure 4

a) SEM image of a Pt/Pd-coated tip array that was not used for writing. The inset is the SEM image of a single polymer pen. b) SEM image of the same pen array taken after 100 writing operations. The inset is the SEM image of a single polymer pen. The scale bar of both figures is 200 μm.