Skip to main content
. 2014 Feb 13;2014:475280. doi: 10.1155/2014/475280

Figure 7.

Figure 7

Degradation of PLGA/chitosan and PLGA nanofibers: (a) comparing the mass loss percentage at different time points, (b) and (c) SEM image of PLGA/chitosan and PLGA nanofibers, respectively, after 14 days of incubation in PBS solution at 37°C.