The content of emulsion electrospinning solutions and the electrospun nanofibers.

Sample number PLGA conc.
(w/v)
Chitosan conc.
(w/v)
PVA conc.
(w/v)
Total emulsion conc.
(w/v)
PLGA (%W) after and before PVA removal Chitosan (%W) after and before PVA removal
1 20 4 8 10.6 84 (62.5) 16 (12.5)
2 16 4 8 9.3 80 (57) 20 (14.3)
3 12 4 8 8 75 (50) 25 (16.7)
4 20 6 8 11.3 77 (60) 23 (17.6)
5 16 6 8 10 73 (53) 27 (20)
6 12 6 8 8.6 67 (46) 33 (25)