Figure 5.

Figure 5

Graph of AFM force mapping results. Error bars are standard deviations; n=3 for each film type. BIS/pDADMAC untreated vs. BIS/pDADMAC crosslink-treated, p = 0.012; BIS/PEI untreated vs. BIS/PEI crosslink-treated, p = 0.017