Table 2.
Stage I (°C) | Stage II (°C) | Stage III (°C) | Stage IV (°C) | Screw speed (pr/min) | Macroscopic morphology of film |
---|---|---|---|---|---|
100 | 140 | 140 | 130 | 40 | Film with white points |
110 | 150 | 150 | 137 | 40 | Smooth film |
120 | 160 | 160 | 140 | 40 | Unformed film |
110 | 150 | 150 | 137 | 20 | Unformed film |
110 | 150 | 150 | 137 | 60 | Porous film |