Table 1: Type of material, method of polymerization and polymerization cycle used.

Group Material Brand Method Polymerization Cycle
1 Heat cure denture base resin DPI Plain Heat Water bath polymerization – 74oC for 2 hours and 100oC for 1 hour6
2 Heat cure denture base resin Acralyn HCrosslinked Heat Water bath polymerization – 74oC for 2 hours and 100oC for 1 hour6
3 Heat cure denture base resin DPI Plain Microwave Microwave polymerization – 13 minutes at 85 to 100 Watts and 90 seconds at 500 Watts36,45
4 Heat cure denture base resin Acralyn HCrosslinked Microwave Microwave polymerization – 13 minutes at 85 to 100 Watts and 90 seconds at 500 Watts36,45