Skip to main content
. 2013 Oct 18;5(4):183–190. doi: 10.1038/ijos.2013.73

Table 3. Wear results of the teeth and their opposing crowns obtained in the reviewed studies.

Studies Results, mean wear (s.d.)
Occlusal wear of ceramic crowns Occlusal wear of opposing natural teeth
Suputta-mongkol 2008    
 Wear volume/mm3 Premolar 0.19 (0.06) Premolar 0.21 (0.06)
  Molar 0.34 (0.08) Molar 0.50 (0.22)
 Wear height/µm Premolar 29 (12) Premolar 46 (13)
  Molar 36 (34) Molar 65 (29)
Etman 2008    
 Procera    
  Wear in µm after 6 months 143.60 (9.47) 130.96 (15.08)
  Wear in µm after 12 months 201.18 (0.22) 184.24 (15.02)
  Wear in µm after 18 months 243.70 (7.31) 216.84 (14.14)
  Wear in µm after 24 months 321.60 (12.79) 261.58 (12.88)
 Experimental ceramic    
  Wear in µm after 6 months 108.50 (4.87) 102.02 (8.49)
  Wear in µm after 12 months 148.16 (6.38) 149.7 (6.59)
  Wear in µm after 18 months 194.18 (11.92) 193.92 (12.07)
  Wear in µm after 24 months 214.76 (4.9) 214.86 (6.09)
 MC    
  Wear in µm after 6 months 87.06 (2.96) 75.52 (7.15)
  Wear in µm after 12 months 116.3 (4.70) 106.9 (10.19)
  Wear in µm after 18 months 142.30 (3.91) 133.82 (6.94)
  Wear in µm after 24 months 176 (3.93) 156.42 (14.34)
Silva 2011 (at year 3 in mm3)    
 MC 1.48 (0.20) 1.10 (0.10)
 IPS e.max Press without veneering 1.06 (0.12) 0.80 (0.09)
 IPS Empress 2/IPS Eris ceramic 1.31 (0.17) 1.02 (0.20)

s.d., standard deviation.