Figure 1. Illustration of the synthesis procedure of the Pd/RGO catalysts.

Figure 1

GO is dissolved in NMP and formed uniformly solution; Then Pd(acac)2, OAm and TOP are added into mixed solution and heated to 200°C for 2 hours; Finally, monodisperse Pd NPs are formed on the surface of RGO.