Table 3.
Electrospun time, min | 2PU10GE | 4PU10GE | 6PU10GE | 8PU10GE | |
---|---|---|---|---|---|
Fibre Diameter (μm) | 0.54±0.06 | 1.04±0.10 | 1.15±0.13 | 1.22±0.11 | |
Fibre Bulk density (g/cm3) | - | 1.34 | 1.34 | 1.32 | |
Membrane Thickness (μm) | 10 | 21.6±4.0 | 23.4±2.6 | 25.1±5.2 | 22.2±14.0 |
40 | 56.8±4.9 | 40.3±5.7 | 36.0±5.4 | 67.7±6.7 | |
Fibre packing density (g/cm3) | 10 | 0.285±0.068 | 0.276±0.009 | 0.257±0.066 | 0.214±0.079 |
40 | 0.595±0.045 | 0.539±0.057 | 0.474±0.017 | 0.469±0.056 | |
Porosity (%) | 10 | - | 79.4 2±0.63 | 80.79±4.93 | 83.84±6.0 |
40 | - | 59.78±4.29 | 64.51±1.3 | 64.51±4.25 |