Figure 3. Longitudinal (black) and Hall (red) magnetoresistivity at a temperature T = 1.6 K measured in a (30 × 280 μm2) Hall bar geometry in graphene samples as-grown and after hydrogenation.

Figure 3

a) Pristine graphene layer (Sample A) b) Pristine graphene Layer (Sample B) c) Graphene layer after hydrogenation (Sample BH2).