Skip to main content
. Author manuscript; available in PMC: 2014 Apr 2.
Published in final edited form as: J Biomed Mater Res A. 2011 Jan 25;96(4):682–692. doi: 10.1002/jbm.a.33024

TABLE I.

Effect of Immobilized GAGs on Cell Viability

Cell Viability (%)
Culture Surface Day 7 Day 11 Day 14 Day 17
Polystyrene control 83.9 ± 2.6 72.0 ± 1.8 70.0 ± 1.8 41.2 ± 3.6
Chitosan control 84.6 ± 0.8 73.2 ± 2.2 70.8 ± 7.1 39.9 ± 6.0
Heparin 94.6 ± 0.3a,b 81.7 ± 1.4a,b 75.2 ± 7.3 58.0 ± 4.0a,b
Dermatan sulfate 90.1 ± 1.9a,b 80.8 ± 1.0a,b 70.0 ± 3.5 48.8 ± 4.3
Hyaluronan 84.0 ± 0.6 75.3 ± 2.9 70.4 ± 4.8 38.6 ± 7.9
Heparan sulfate 93.9 ± 1.0a,b 79.9 ± 2.8a,b 73.4 ± 5.1 57.4 ± 2.6a,b
a

Comparison with polystyrene surface, p < 0.05.

b

Comparison with chitosan surface, p < 0.05.