Published in final edited form as: J Biomed Mater Res A. 2011 Jan 25;96(4):682–692. doi: 10.1002/jbm.a.33024

TABLE II.

Effect of Immobilized GAGs on Total Mk Fraction

Total Mk Fraction (%)
Culture Surface Day 7 Day 11 Day 14 Day 17
Polystyrene control 16.8 ± 3.8 37.8 ± 9.8 69.7 ± 2.9 70.3 ± 1.2
Chitosan control 18.3 ± 4.1 43.4 ± 14.2 75.0 ± 2.5a 72.9 ± 5.1
Heparin 19.7 ± 4.9 45.5 ± 18.1 78.3 ± 5.5a 69.7 ± 8.0
Dermatan sulfate 18.3 ± 3.4 47.4 ± 19.5 76.9 ± 3.4a 72.8 ± 4.5
Hyaluronan 19.9 ± 6.1 42.7 ± 16.1 73.9 ± 2.2a 69.2 ± 2.1
Heparan sulfate 20.2 ± 5.1 47.5 ± 19.8 76.5 ± 2.0a 69.2 ± 4.7
a

Comparison with polystyrene surface, p < 0.05.