Figure 1.

Figure 1.

(a,b) Bioactive ceramic (TCP) scaffolds fabricated by SLS; (c) Micro/nanometer-sized porous morphology; and (d) Pore size distribution curve on the etched surface of HAP/TCP (60/40 w/w) ceramic scaffold.