Published in final edited form as: J Biomed Mater Res A. 2013 Oct 12;102(9):3102–3111. doi: 10.1002/jbm.a.34983

Fig. 5. Micro-CT images.

Fig. 5

Representative 3D reconstructed images after 8 weeks of: A- Empty defects; B – SPCL scaffolds alone; C – SPCL scaffolds with ASCs. Black bar represents 5.0 mm. D – Chart representing percentage of mineralized tissue present on total area of the defects (ROI was determined covering the entire defect area) (n = 3 defects per group). Values presented as mean ± SD. Significance measured by one-way ANOVA where ** represents p < 0.01.