Skip to main content
. 2014 Mar 21;39(2):89–94. doi: 10.5395/rde.2014.39.2.89

Table 3.

Compressive strength (MPa) of test materials

graphic file with name rde-39-89-i003.jpg

Values are expressed as mean ± standard deviation (n = 10 for each group).

Different superscript upper-case letters indicate a statistically significant difference among the materials (p < 0.05) and different superscript lower-case letters indicate a statistically significant difference between different time points (p < 0.05).

MTA, mineral trioxide aggregate; BA, Bioaggregate; BD, Biodentine.