Table 1.

Surface treatments carried out on alloy test samples and mean loads at fracture

Group No. Surface treatment Mean (Mpa)
I Sandblast + surface grinding 23.6
II Sandblast + surface grinding + sandblast 30.7
III Sandblast + surface grinding + sandblast + de-gas 37.9
IV Sandblast + surface grinding + sandblast +de-gas + sandblast 36.0
V Sandblast + surface grinding + sandblast + de-gas + surface grinding + sandblast 27.5
VI Sandblast + surface grinding + sandblast + de-gas + surface grinding + sandblast + de-gas 28.4
VII Sandblast + surface grinding + sandblast + steam clean + de-gas 20.77