Skip to main content
. 2014 Apr 16;7:8. doi: 10.3389/fneng.2014.00008

Table 1.

Electrochemical characterization of HSA coatings.

|Z| @ 100 Hz [Ω] |Z| @ 1 kHz [Ω] CTCtot1[mC cm-2] CTCtot2[mC cm-2]
PEDOT-agar 142.6 ± 1.7 139.5 ± 1.6 149.7 ± 7.3 246.2 ± 4.9
PEDOT-CNT 127.6 ± 0.1 125.0 ± 0.2 92.3 ± 4.6 158.7 ± 8.2
PPy-CNT 138.7 ± 4.3 136.7 ± 4.1 67.7 ± 0.5 118.9 ± 4.8
Au-agar 291 ± 12 214.6 ± 8.3 3.1 ± 0.7 6.2 ± 0.5
Au-CNT 334 ± 50 192 ± 25 2.5 ± 0.3 4.6 ± 0.2
Uncoated 1915 ± 203 441 ± 7 0.5 ± 0.1 3.3 ± 0.2