Published in final edited form as: Dent Mater. 2013 Dec 13;30(2):227–233. doi: 10.1016/j.dental.2013.11.007

Table 2.

Total MMP activity (absorbance) detected in completely demineralized dentin specimens before and after the application of different cross-linking solutions for 30 s or 60 s.

Dentin treatment Application time

30 s 60 s


Initial MMP activity Post-treatment MMP activity Initial MMP activity Post-treatment MMP activity
Water 0.227 (0.146–0.279)*a 0.265 (0.235–0.334)a 0.255 (0.225–0.302)a 0.232 (0.176–0.239)a
0.5 M EDC 0.183 (0.157–0.229)a 0.095 (0.072–0.106)b 0.378 (0.332–0.426)a 0.100 (0.070–0.160)b
1 M EDC 0.255 (0.240–0.319)a 0.136 (0.085–0.173)b 0.266 (0.236–0.311)a 0.052 (0.045–0.079)b
2 M EDC 0.252 (0.236–0.279)a 0.095 (0.077–0.102)b 0.241 (0.194–0.260)a 0.042 (0.034–0.061)b
10% GA 0.183 (0.141–0.209)a 0.092 (0.078–0.108)b 0.384 (0.318–0.492)a 0.105 (0.100–0.120)b
*

Values are expressed as absorbance at 412 nm after 60 min of incubation in SensoLyte substrate and represent median values (25 percentile–75 percentile), n = 10.

Within each dentin treatment and application time (initial vs after-treatment MMP activity), medians identified by the same letter are not statistically different (Wilcoxon, p > 0.05).