Showing mean difference in surface roughness (R a, μm) among various subgroups of group I—conventional glass ionomer cement (GC Fuji II).

Subgroup Subgroup Surface roughness (R a, μm)
Mean difference (P value) Significance
Subgroup IA (Control) Subgroup IB −0.11 <0.001 HS
Subgroup IC −0.28 <0.001 HS
Subgroup ID −0.97 <0.001 HS
Subgroup IE −1.38 <0.001 HS