Skip to main content
. 2014 Apr 28;2:21. doi: 10.3389/fchem.2014.00021

Figure 6.

Figure 6

(A) Representative fitting curves for 10 wt% RLP and 10 wt% 4-arm PEG hydrogels; (B) summary of relaxation rate of 5 wt% (square), 10 wt% (diamond) and 20 wt% (triangle) RLP and 10 wt% 4-arm PEG (circle) hydrogels at 15, 45, and 90% constant strains. The stress relaxation behavior was fitted to an exponential equation: σ (t) = σo + A* exp(− tκ), where σo is the offset shear stress, A is the decay amplitude and κ is the relaxation rate. Error bars represent the standard deviation of three measurements.