Skip to main content
. 2014 May 6;4:4849. doi: 10.1038/srep04849

Figure 2. Time-dependent evolution of the products.

Figure 2

SEM images of the particle surfaces obtained at different galvanic reaction time (a) 10 min, a porous Au particle layer formed at the surface of Cu2O, (b) 1 h, trace of second porous layer formed on the top of the first porous Au layer, (c) 6 h, clear second porous layer formed, (d) 12 h, 3D porous Au structure formed.