Figure 6.
SEM micrographs of LBL coating degradation. Titanium rods coated with a LBL process using D32-135, were imaged at various time points over a 3 week incubation in PBS containing 0.05% BSA at 37°C. Scale bar = 3 μm
SEM micrographs of LBL coating degradation. Titanium rods coated with a LBL process using D32-135, were imaged at various time points over a 3 week incubation in PBS containing 0.05% BSA at 37°C. Scale bar = 3 μm